Question details (Specific performance):Biomass environmental protection and energy saving fuel made of straw and livestock etc., their combustion is not full. Answer: The cause of the problem:1. Air quantity is insufficient or too big.2. Outer flame position is not proper.Troubleshooting:1.Sufficient temperature: sufficient combustion of biomass boiler needs high temperature, combustion rate is proportional to the temperature, to raise the temperature as much as possible but guarantee there is no slagging.2. Proper air volume. If the air volume is too large, it will reduce the temperature of the furnace and increase the incomplete combustion of fuel. If the air volume is insufficient, the combustion efficiency will be reduced, and the waste of fuel will also increase the emission of smoke.3. Sufficient mixing of fuel and air. During the burning stage of biomass boilers, the sufficient mixing of air and fuel should be ensured and the disturbance should be strengthened during the burnin
(Question Details) Specific Performance:The pipe of superheater bursts in circulating fluidized bed boiler operation.The bed pressure indicator fluctuates little. Answer: causes of failure:(1) Design Factors.(2) Manufacturing process, installation and maintenance quality.(3) The temperature control device is unreasonable or does not work properly.(4) Effect of operating conditions on overheating and explosion of superheater. Troubleshooting:(1) Report the fact to operator on duty and require operating the boiler in low load.(2) When the overheat damage is serious,please report it to operator on duty and require stoping the boiler immediately to prevent blowout of the near pipes.(3) Adjust the steam temperature as much as possible within the normal range.(4) If the superheater tube is not damaged badly, it has little effect on the temperature level of the steam, and it can be allowed to run in a low load range for a short period of time.
(Question Details) Specific Performance:(1) The bed temperature has risen sharply.(2) The oxygen level drops even to zero.(3) The current of the primary blower is reduced, and the wind pressure in the wind chamber is high and fluctuates.(4) The furnace negative pressure increases and the induced draft fan current decreases.(5) Difficulties in slagging.(6) If coking in low temperature, the bed temperature, bed pressure distribution is uneven, the deviation is too large, the bed pressure, the plenum pressure, the bed temperature is not normal, and the local bed temperature measurement point is not normally raised or lowered.(7) The bed pressure indicator value fluctuates little. Answer: causes of failure :(1) Improper operation, resulting in overheated bed temperature and coking.(2) The primary air volume during operation is kept too small, which is lower than the minimum fluidized air volume, so that the material can’t be well fluidized but piled up, the temperature field of the entire
(Details on the problem) Specific Performance:Slagging pipe blocks during operation of circulating fluidized bed boiler. Answer:cause of failure:(1) The internal shape is caused by the limited expansion of the wear-resistant material inside the slag discharge pipe. The internal components of the slag cooler are deformed, affecting the fluidization of the slag cooler; the slag cooler is deactivated for a long time or a single slag cooler is selected for slagging, and the bed material in the deactivated slag cooler is bonded under the influence of steam, which being low temperature coke.(2) The operating personnel did not grasp the ratio of the fluidized air volume of the slag cooler. Inappropriate air volume ratio resulted in poor ash slag fluidization in the slag cooler. Troubleshooting:(1) Operation personnel should strengthen understanding of boiler operating conditions, adjust boiler parameters in a timely manner, set up the concept of boiler material dynamic balance, control boiler
(Question Details) Specific Performance:(1) There are blasting sounds in the furnace, and the furnace chamber is under positive pressure. There is smoke emitted from the combustion chamber in a leakage. In severe cases, the explosion-proof door of the boiler body opens.(2) Drum water level drops rapidly and the feedwater flow rate is not abnormally larger than steam flow. MFT acts when the water level is below -280mm.(3) Drum pressure, steam flow rate, exhaust temperature decrease, smoke temperature difference increases on both sides.(4) The negative pressure at the inlet of the flue and suction fan becomes smaller and the temperature difference between the two sides increased. (5) Smoke temperature decreases at the inlet and outlet of the cyclone separator, and the temperature of the material returned is low.(6) Bed pressure increases, bed materials clean, fluidization poof, bed temperature distributes unevenly and bottom slag discharge difficultly. Answer:cause of failure:(1) Fly ash
Question details (Performance):1. High temperature of motor, fast temperature rise.2. Overload, high outlet pressure and frequent safety valve open often.3. The vibration is intensified, the side vibration of the fan motor coupling is large, and the fan body never vibrates to vibration.4. No obvious vibration was found in no-load test of fan motor. Answer: Fault reason:Fan bearing vibration is common fault in the operation, the vibration of the fan will cause damage of bearing and blade, bolt looseness, chassis and wind damage, fan vibration rises abruptly in the operation. this is because when the gas enter impeller and the rotating blade working face has certain angle, according to the principle of fluid mechanics, gas from non-working face must be a spiral blade, so the dust particles in the gas will slowly sedimentation due to vortex. Airfoil blades are very easy to accumulate dust. When the accumulated ash reaches a certain weight, a part of the large amount of accumulated ash wi
(Question details) Specific performance:The wall thickness of several boiler tubes was significantly reduced in a large area, the remaining wall thickness was 2.0mm, and some furnace tubes were corroded and worn out. Furnace tube wall is covered with a thick layer of uneven scale, the surface of the scale is brick red and black, scale layer is loose, and it is easy to remove the inner wall of the furnace tube, after removing, the furnace tube wall covered with a layer of corrosion pits. There is a thin layer of brick red corrosion on the outer wall of boiler tube, some of which are attached with black adhesive. Answer: Fault reason:1. The boiler is seriously short of water.2. Poor water circulation and uneven combustion.3. The unqualified quality of the boiler water and undemanding chemical supervision make the inner wall of the pipe corrode and scale, causing the pipe overheat and reduction of the strength.4. Due to the presence of impurities and scale, the furnace tube is blocked ins
Question details (performance):A pump in a gas boiler does not transfer oil. Answer: Fault reason:(1) Pump failure.(2) Oil pressure and power are reduced.(3) The oil inlet valve is not sealed.(4) The inlet pipe is not sealed.(5) The interceptor valve is closed.(6) The filter is contaminated.(7) The filter is not sealed.(8) The tubing is not sealed.(9) Pump suck air inlet.(10) The vacuum degree in oil tube is too high.Troubleshooting:(1) Replace with new pump.(2) Remove the inlet valve and clean or replace it.(3) Seal the inlet pipe.(4) Open.(5) Cleaning.(6) Replace the sealing ring.(7) Tighten and exhaust.(8) Clean the filter and valve.