(Question Details) Specific Performance:(1) The bed temperature has risen sharply.(2) The oxygen level drops even to zero.(3) The current of the primary blower is reduced, and the wind pressure in the wind chamber is high and fluctuates.(4) The furnace negative pressure increases and the induced draft fan current decreases.(5) Difficulties in slagging.(6) If coking in low temperature, the bed temperature, bed pressure distribution is uneven, the deviation is too large, the bed pressure, the plenum pressure, the bed temperature is not normal, and the local bed temperature measurement point is not normally raised or lowered.(7) The bed pressure indicator value fluctuates little. Answer: causes of failure :(1) Improper operation, resulting in overheated bed temperature and coking.(2) The primary air volume during operation is kept too small, which is lower than the minimum fluidized air volume, so that the material can’t be well fluidized but piled up, the temperature field of the entire
(Question details) Specific performance:The wall thickness of several boiler tubes was significantly reduced in a large area, the remaining wall thickness was 2.0mm, and some furnace tubes were corroded and worn out. Furnace tube wall is covered with a thick layer of uneven scale, the surface of the scale is brick red and black, scale layer is loose, and it is easy to remove the inner wall of the furnace tube, after removing, the furnace tube wall covered with a layer of corrosion pits. There is a thin layer of brick red corrosion on the outer wall of boiler tube, some of which are attached with black adhesive. Answer: Fault reason:1. The boiler is seriously short of water.2. Poor water circulation and uneven combustion.3. The unqualified quality of the boiler water and undemanding chemical supervision make the inner wall of the pipe corrode and scale, causing the pipe overheat and reduction of the strength.4. Due to the presence of impurities and scale, the furnace tube is blocked ins